I just wrapped up a production run in the workshop focusing on the precise interaction between dense cotton-polyester substrates and Direct to Film inks. By holding the pre-curing stage at exactly 115°C for 90 seconds, the resin reaches full gelation, ensuring the print remains crack-free and flexible.
#TextileEngineering #DTFPrinting #ApparelManufacturing #TextileWorkshop #DragonEburneo
I just wrapped up a production run in the workshop focusing on the precise interaction between dense cotton-polyester substrates and Direct to Film inks. By holding the pre-curing stage at exactly 115°C for 90 seconds, the resin reaches full gelation, ensuring the print remains crack-free and flexible.